Causes of Mold Adhesion During Rubber Molding and Their Solutions


Multi-line text content element

HTML language content can be parsed after rich text content is bound to data

Release time:

Sep 30,2026

Abstract:
After vulcanization, molded rubber products often adhere to the mold and are difficult to demold, which is one of the most challenging issues in rubber processing and directly affects product quality, appearance, and production efficiency. This paper systematically analyzes the causes and mechanisms of mold adhesion from multiple perspectives, including hydrogen‑bonding adsorption of surface hydroxyl groups on white fillers (precipitated silica), under‑vulcanization, excessive use of resins, adhesives, or metal salts in the compound, mold‑related factors, as well as the vulcanization system and process parameters. Drawing on both domestic and international literature and industry practice, the study proposes comprehensive solutions, such as formulation optimization, mold treatment, process adjustments, and the application of release agents.


I. Introduction:
During the rubber compression molding and vulcanization process, adhesion between the molded part and the mold is a complex physicochemical issue. As a polymeric material, rubber inherently exhibits poor adhesion to highly polar metallic surfaces; even when using highly polar rubbers—whose intrinsic mechanical strength often exceeds the adhesive forces between rubber and metal—the risk of severe mold sticking remains relatively low. Nevertheless, in actual production, mold‑sticking is a common occurrence, and in severe cases can result in parts that cannot be demolded or in product tearing caused by forced removal. The factors contributing to this problem are highly intricate, encompassing aspects such as formulation design, filler selection, vulcanization conditions, and the condition of the mold itself.


II. Excessive white filler (precipitated silica) — hydrogen bonding and hydroxyl group adsorption:
2.1 Chemical Adsorption Properties of Surface Hydroxyl Groups on White Carbon Black
Precipitated or fumed silica, commonly referred to as white carbon black, possesses a large number of silanol groups (≡Si–OH) on its surface. These hydroxyl groups exhibit exceptionally strong chemical adsorption activity. The silanol groups on the silica surface associate via hydrogen bonding, thereby enhancing interparticle interactions; meanwhile, their poor compatibility with rubber molecules limits the extent of intimate contact between the silica and the rubber matrix.
During vulcanization, the hydroxyl groups on precipitated silica exhibit strong polarity and, at elevated temperatures, readily interact with the oxide layer on the metal mold surface—sometimes even forming covalent bonds—thereby giving rise to sticking problems. Moreover, the hydroxyl groups between precipitated silica particles can establish a hydrogen-bonding network, increasing the compound’s viscosity; this type of interaction is remarkably robust.
2.2 Acidity of precipitated silica and its interference with vulcanization
Ordinary precipitated silica is acidic and tends to adsorb vulcanizing agents, thereby reducing vulcanization efficiency—mold sticking often indicates an insufficient degree of cure. Precipitated silica also absorbs free water from the rubber compound, further interfering with the vulcanization reaction. When peroxide systems encounter precipitated silica, mold‑sticking becomes particularly pronounced.
2.3 Solution
(1) Silane coupling agent modification. This is the most fundamental approach to addressing the problem of silica agglomeration and mold sticking. The silane coupling agent reacts with the surface hydroxyl groups of precipitated silica, transforming its hydrophilic nature into hydrophobicity, thereby enhancing its compatibility with rubber and improving its dispersibility. Commonly used silane coupling agents such as Si69 and Si50 can react with the silanol groups on the silica surface, forming long-chain structures—silica–silane–rubber—that eliminate hydrogen bonding and electrostatic adsorption between filler particles.
(2) Addition of structuring agents. For silicone rubber systems, structuring agents such as hydroxyl‑terminated silicone oil, diphenylsilanediol, or alkoxy‑terminated silanes can be incorporated to pre‑modify the surface of precipitated silica, removing a portion of its surface hydroxyl groups and thereby reducing the number of reactive sites on the silica.
(3) Control the dosage of precipitated silica. If mold sticking is indeed caused by precipitated silica, the amount of precipitated silica used should be appropriately reduced.
(4) Use white carbon black activators. Incorporate white carbon black activators such as PEG (polyethylene glycol) and DEG (diethylene glycol) into the formulation to enhance the compatibility between white carbon black and rubber.


III. Sulfur Deficiency—The Primary Cause of Sticking to the Mold:
3.1 Mechanism of Mold Sticking Caused by Sulfur Deficiency
Insufficient vulcanization is the primary cause of sticking to the mold. When the vulcanization time is inadequate, the vulcanization temperature is too low, or the amount of vulcanizing agent is insufficient, the crosslink density of the rubber fails to reach the optimum level, resulting in excessively low compound strength; consequently, the compound tears and remains stuck inside the mold upon demolding.
Contaminants within the mold, combined with severely over‑cured or slightly carbonized rubber molecules adhering to its surface, decompose during vulcanization into acids, aldehydes, ketones, water, and plasticizers. These decomposition products increase the polarity of the polymer material. Moreover, these residues still contain significant amounts of rubber hydrocarbons or organic compounds, which continue to exhibit strong adhesion to or crosslinking with the rubber. Consequently, when the next molding cycle is under‑cured, the rubber compound is torn apart inside the mold.
In winter, when ambient temperatures are low, the mold temperature drops rapidly after opening, making under‑curing and sticking to the mold more likely.
3.2 Solution
(1) Ensure proper vulcanization. Preventing continuous under‑vulcanization is the top priority. The optimum vulcanization time (t90) should be determined using a vulcanization curve—such as that obtained with a rubber process analyzer (RPA)—and the vulcanization process must be strictly controlled in accordance with this parameter.
(2) Optimize vulcanization temperature and time. For products experiencing mold sticking, first try extending the vulcanization time or increasing the vulcanization temperature. In peroxide‑cured systems, excessively low mold temperatures can lead to residual peroxides, causing mold adhesion; raising the vulcanization temperature can significantly mitigate this issue.
(3) Check the uniformity of equipment temperature. The temperature deviation of the flat‑plate vulcanizing press should be inspected regularly; uneven temperature can lead to localized under‑vulcanization.
(4) Enhance the hot tear strength of the rubber compound. By optimizing the formulation, the hot tear strength of the compound can be improved, reducing the likelihood of it tearing within the mold during demolding.


4. Excessive amounts of resin, adhesives, or metal salts in the rubber compound:
4.1 Influence of Resins and Adhesives
Resins (such as phenolic resins) and adhesives (such as isocyanates and cobalt salts) used in certain rubber formulations exhibit strong polarity; their mechanism relies on this pronounced polarity to enhance interphase penetration, mutual diffusion, and adsorption. When these components are present in excessive amounts, they can markedly increase the adhesive forces between the rubber and the metal mold, leading to sticking.
4.2 Effects of Metal Salts
Although certain metal salts, such as zinc stearate, are commonly used as internal release agents in formulations, their dosage must be carefully controlled. Zinc stearate exhibits very low solubility in rubber and tends to migrate to the surface. A typical usage level of 1–2% is considered safe; exceeding this range can lead to excessive surface migration. Moreover, if the plasticizing effect is too pronounced—resulting from an excessive amount of zinc stearate—it may adversely affect the rubber’s physical and mechanical properties, leading to a reduction in tensile strength.
In addition, metal salt byproducts formed when certain accelerators react with activators can also cause mold contamination and sticking. Some literature indicates that zinc oxide and stearic acid can corrode molds, and recommends replacing part of the zinc oxide and stearic acid with zinc stearate.
4.3 Solution
(1) Strictly control the dosage of resins and adhesives. While ensuring that bonding performance requirements are met, minimize the amount of polar resins and adhesives added.
(2) Control the dosage of metal salts. The amount of internal release agents such as zinc stearate should be kept within 1–2 parts to prevent excessive dosing, which can lead to blooming and reduced mechanical strength.
(3) Properly formulate the activator system. The amount of zinc oxide should be moderate, avoiding excess while ensuring adequate vulcanization activity.


V. Over‑sulfurization and Reversion of Vulcanization:
5.1 Mechanism of Mold Sticking Caused by Over‑vulcanization
Over‑vulcanization can also lead to sticking to the mold. Excessive sulfur crosslinking renders the rubber compound brittle; when the mold is opened, such brittle material is prone to cracking, leaving small fragments on the mold surface. Over time, these residues accumulate and exacerbate mold sticking. For natural rubber and similar elastomers, over‑vulcanization may further cause reversion, resulting in a tacky, softened surface.
5.2 Solution
(1) Precisely control the vulcanization time. To avoid excessive vulcanization, demolding should be carried out near the optimum cure point.
(2) Select a vulcanization system that is resistant to reversion. For thick‑walled products or high‑temperature vulcanization processes, an anti‑reversion agent or an effective vulcanization (EV) system may be employed.
(3) Clean the mold promptly. As soon as any rubber residue is detected, the mold should be cleaned immediately to prevent buildup.


VI. Mold-related factors:
6.1 Mold Material and Surface Finish
Mold material and surface finish are critical factors affecting demolding. Low‑quality steel can exacerbate sticking. An excessively rough mold surface increases the contact area and mechanical interlocking between the rubber and the mold, making demolding more difficult. Conversely, an overly smooth mold surface—such as a mirror finish—can also lead to increased adhesion due to enhanced intermolecular forces.
Contaminants and deposits on the mold surface are direct causes of sticking. During rubber vulcanization, these residues can adhere to or crosslink with the rubber.
6.2 Solution
(1) Select high-quality mold steel. Choose mold steels that exhibit excellent corrosion resistance and thermal stability.
(2) Mold surface treatment. Electroplating the mold (e.g., chrome plating) is an effective anti‑sticking measure. In addition, the mold surface can be treated with PVD coating, FEP coating, or sol–gel coating. Studies have shown that sol–gel coatings, composed of oxygen, silicon, carbon, and titanium, exhibit excellent film‑forming properties, with a sulfurization release force of approximately 20 N—comparable to that of PTFE coatings. Compared with molds made of 45 steel, such coatings enable about 300 additional sulfurizations, thereby increasing the mold’s continuous service life by a factor of 2 to 3.
(3) Clean the mold regularly. Depending on the degree of contamination, clean the mold periodically with a mold‑cleaning solution. However, be aware that high‑temperature cleaning solutions can corrode the mold, leaving it more rough; therefore, do not resume production immediately after cleaning.
(4) Sandblasting or roughening of the mold. For molds with severe corrosion, it is necessary to perform sandblasting or electroplating prior to further processing.


VII. Vulcanization System and Process Parameters:
7.1 Characteristics of Peroxide Systems
The peroxide vulcanization system exhibits particularly severe mold‑sticking issues when used with precipitated silica. Peroxides are highly sensitive to the acidity of the formulation. When employing a peroxide‑based system, the following adjustments may be considered:
Select peroxides with a lower half-life temperature to accelerate the vulcanization rate.
A crosslinking aid such as TMPTMA or HVA‑2 can be used in place of TAIC, resulting in a faster vulcanization rate.
Avoid using peroxides in combination with sulfur to prevent off‑odors and mold‑adhesion issues.
7.2 Mixing Process
Uneven mixing can lead to uneven dispersion of the vulcanizing agent, resulting in inconsistent local degrees of vulcanization and causing sticking to the mold. Over‑mixing, on the other hand, reduces the compound’s strength and increases its tendency to stick to the mold. It is essential to ensure:
Uniform mixing and good dispersion of the vulcanizing agent.
Avoid over‑vulcanization, which can reduce the compound’s strength.
The rubber content should not be too low.


VIII. Application of Release Agents:
8.1 External Release Agent
Spraying or brushing an external release agent onto the mold surface is the most straightforward method for preventing sticking. However, please note:
Although spray‑on silicone oil can address demolding issues, it may give rise to new defects such as surface oil contamination, flow marks, localized sponge‑like areas, and bubbles.
External release agents must be applied frequently and evenly.
Some argue that simply spraying an external release agent to address mold‑sticking is the least advisable solution.
8.2 Internal Release Agent
Adding an internal release agent to the rubber compound can improve its flow. During processing, the lubricant readily migrates from the interior of the compound to the surface, forming an extremely thin “lubricant molecular layer” that reduces friction between the rubber and the mold. Common internal release agents include:
Metal soaps such as stearic acid and zinc stearate
Specialized internal release agents, such as IM-1 and AT-16-Ⅲ, etc.
The dosage of internal release agent should be moderate; excessive use may result in blooming.
Mold‑pressing rubber vulcanization adhesion to molds is a complex issue involving multiple interrelated factors. Hydrogen bonding of surface hydroxyl groups on white fillers (precipitated silica) constitutes the core mechanism underlying filler‑related adhesion; solutions lie in silane coupling‑agent modification and careful control of filler structure. Under‑vulcanization is the primary process‑control concern, with achieving proper vulcanization as the fundamental requirement. Excessive resin, adhesive, or metal salts necessitate precise formulation design and rigorous control. Moreover, mold material and surface treatment must not be overlooked.
In actual production, a systematic troubleshooting approach is essential. Comprehensive process control—from formulation design (including filler selection and modification, as well as precise adjustment of additive dosages), to vulcanization parameters (with meticulous regulation of temperature, time, and pressure), to mold management (covering material selection, surface treatment, and routine cleaning), and finally to release agent application (employing both internal and external treatments in appropriate amounts)—is required to effectively address the persistent issue of mold sticking. As industry experts emphasize: “Preventing continuous under‑curing is the top priority; selecting high‑quality steel, electroplating the molds, and enhancing the thermal tear strength of the rubber compound are all critical.” In short, formulation, processing, and tooling must be integrated as an inseparable triad—none can be omitted.